Figure 1

Figure 1. Test pattern images taken with a back-illuminated 2048 x 2048 CCD at –120C. Measured quantum efficiency and (1 – Reflectivity) versus wavelength [7]. CTIO T2k is a thinned CCD (approximately 20 mm thick).